Publications

An investigation on the mechanical properties of soft magnetostrictive FeCoCr films by nanoindentation

Author | Baco S, Abbas QA, Hayward TJ, Morley NA

DOI | https://doi.org/10.1016/j.jallcom.2021.160549

Abstract

DOI | https://doi.org/10.1016/j.jallcom.2021.160549